Inhibited buffer-complexing ferrous citrate+citric acid solutions, 2.5<pH<3.5, at 363±5K, is used to dissolve a compact magnetite layer grown on low alloyed steel in a nuclear plant generator. The average rate of oxide dissolution is 40 m/h. Similarly, a compact duplex layer of magnetite covered by hematite formed on a carbon steel pipe of a classical heat exchanger dissolves in less than 10 h. The mean rate of metal uniform corrosion ranges between 1 and 9 mg/cm2 h depending on pH, inhibitors and citrate ion concentration.

  • Collapse
  • Expand

To see the editorial board, please visit the website of Springer Nature.

Manuscript Submission: HERE

For subscription options, please visit the website of Springer Nature.

Journal of Radionalytical and Nuclear Chemistry
Language English
Size A4
Year of
Foundation
1968
Volumes
per Year
1
Issues
per Year
12
Founder Akadémiai Kiadó
Founder's
Address
H-1117 Budapest, Hungary 1516 Budapest, PO Box 245.
Publisher Akadémiai Kiadó
Springer Nature Switzerland AG
Publisher's
Address
H-1117 Budapest, Hungary 1516 Budapest, PO Box 245.
CH-6330 Cham, Switzerland Gewerbestrasse 11.
Responsible
Publisher
Chief Executive Officer, Akadémiai Kiadó
ISSN 0236-5731 (Print)
ISSN 1588-2780 (Online)