Authors:
Hongqiang Qu College of Chemistry and Environmental Science, Hebei University, Baoding 071002, China

Search for other papers by Hongqiang Qu in
Current site
Google Scholar
PubMed
Close
,
Weihong Wu College of Chemistry and Environmental Science, Hebei University, Baoding 071002, China
College of Science, Agricultural University of Hebei, Baoding 071001, China

Search for other papers by Weihong Wu in
Current site
Google Scholar
PubMed
Close
,
Hongjuan Wu College of Chemistry and Environmental Science, Hebei University, Baoding 071002, China

Search for other papers by Hongjuan Wu in
Current site
Google Scholar
PubMed
Close
,
Jixing Xie College of Chemistry and Environmental Science, Hebei University, Baoding 071002, China

Search for other papers by Jixing Xie in
Current site
Google Scholar
PubMed
Close
, and
Jianzhong Xu College of Chemistry and Environmental Science, Hebei University, Baoding 071002, China

Search for other papers by Jianzhong Xu in
Current site
Google Scholar
PubMed
Close
Restricted access

Abstract

The effect of three flame retardants, K2CO3, Na2SiO3·9H2O, and Na2B4O7·10H2O on the process and composition of volatile products of the thermal degradation of wood has been investigated by the thermogravimetric (TG), differential thermogravimetry (DTG), differential thermal analysis (DTA), and the synchronous thermogravimetry–mass spectrometry (TG–MS) analysis methods. The results showed that the ion current intensity and ion peak area of m/z = 18 and 44 MS signals were increased by the flame retardants but the ion peak area of m/z = 28 MS signal was decreased (except K2CO3) at the meantime. What's more, the ion current intensity and ion peak area of m/z = 60 and 68 MS signals were also decreased (except K2CO3), which mean that Na2B4O7 can significantly enhances the dehydration and inhibits the depolymerization of wood. Although K2CO3 accelerates the dehydration reaction, it cannot inhibit the depolymerization reaction effectively, so the flame retardant efficiency of K2CO3 is decreased with the higher concentration. The catalysis of dehydration reaction of Na2SiO3 is the worst one.

  • 1. Gao, M, Sun, CY, Wang, CX. Thermal degradation of wood treated with flame retardants. J Therm Anal Calorim 2006 85 3 765769 .

  • 2. Ondrej, G, Franck, P, Desana, M, Helena, M, Andrea, B. Intumescence in fire retardancy of lignocellulosic panels. Polym Degrad Stab 2003 82:373377 .

    • Crossref
    • Search Google Scholar
    • Export Citation
  • 3. Ergun, B, Mustafa, KY, Mustafa, A, Abdullah, S, Hseyin, P, Mehmet, C. Some physical, biological, mechanical, and fire properties of wood polymer composite (WPC) pretreated with boric acid and borax mixture. Construct Build Mater 2007 21:18791885 .

    • Crossref
    • Search Google Scholar
    • Export Citation
  • 4. Yalinkilic, MK, Takahashi, M, Imamura, Y, Gezer, ED, Demirci, Z, Ilhan, R. Boron addition to non or low formaldehyde cross-linking reagents to enhance biological resistance and dimensional stability for wood. Holz als Roh Werkstoff 1991 57 1 151163.

    • Search Google Scholar
    • Export Citation
  • 5. Chen, PYS, Puttmann, ME, Williams, LH, Stokke, DD. Treatment of hardwood lumber with borate preservation. For Prod J 1997 47 6 6368.

  • 6. Marosi, G, Márton, A, Anna, P, Bertalan, G, Marosfoi, B, Szép, A. Ceramic precursor in flame retardant systems. Polym Degrad Stab 2002 77:259265 .

    • Crossref
    • Search Google Scholar
    • Export Citation
  • 7. Enyu, X, Minxiu, Z Flame retardant science and application 1988 1 National Defence Industry Press Beijing.

  • 8. Silvo, H, Majda, SS, Karin, SK, Marjan, B, Janez, J, Miran, G. Flame retardant activity of SiO2-coated regenerated cellulose fibres. Polym Degrad Stab 2007 92:19571965 .

    • Crossref
    • Search Google Scholar
    • Export Citation
  • 9. Kadir, O, Abdullah, CI, Erol, B, Salih, A. The effect of potassium carbonate borax and wolmanit on the burning characteristics of oriented strandboard (OSB). Construct Build Mater 2007 21:14571462 .

    • Crossref
    • Search Google Scholar
    • Export Citation
  • 10. Dobele, G, Urbanovich, I, Zhurins, A, Kampars, V, Meier, D. Application of analytical pyrolysis for wood fire protection control. J Anal Appl Pyrolysis 2007 79:4751 .

    • Crossref
    • Search Google Scholar
    • Export Citation
  • 11. Liodakis, S, Bakirtzis, D, Dimitrakopoulos, AP. Autoignition and thermogravimetric analysis of forest species treated with fire retardants. Thermochim Acta 2003 399:3142 .

    • Crossref
    • Search Google Scholar
    • Export Citation
  • 12. Franceschi, E, Cascone, I, Nole, D. Thermal, XRD and spectrophotometric study on artificially degraded woods. J Therm Anal Calorim 2008 91 1 119125 .

    • Crossref
    • Search Google Scholar
    • Export Citation
  • 13. Xu, Q, Griffin, GJ, Jiang, Y, Preston, C, Bicknell, AD, Bradbury, GP, White, N. Study of burning behavior of small scale wood crib with cone calorimeter. J Therm Anal Calorim 2008 91 3 787790 .

    • Crossref
    • Search Google Scholar
    • Export Citation
  • 14. Streibel, T, Geißler, R, Saraji-Bozorgzad, M, Sklorz, M, Kaisersberger, E, Denner, T, Zimmermann, R. Evolved gas analysis (EGA) in TG and DSC with single photonionisation mass spectrometry (SPI-MS): molecular organic signatures from pyrolysis of soft and hard wood, coal, crude oil and ABS polymer. J Therm Anal Calorim 2009 96:795804 .

    • Crossref
    • Search Google Scholar
    • Export Citation
  • 15. Tzamtzis, N, Liodakis, S, Pappa, A, Statheropoulos, M, Parissakis, G. The effect of (NH4)2HPO4 and (NH4)2SO4 on the composition of volatile organic pyrolysis products of cellulose: PY-GC studies. Polym Degrad Stab 1997 56:287290 .

    • Crossref
    • Search Google Scholar
    • Export Citation
  • 16. Qu, HQ, Wu, WH, Jiao, YH, Xu, JZ. Thermal behavior and flame retardancy of flexible PVC treated with Al(OH)3 and ZnO. Polym Int 2005 54:14691473 .

  • 17. Liodakis, S, Bakirtzis, D, Dimitrakopoulos, A. Ignition characteristics of forest species in relation to thermal analysis data. Thermochim Acta 2002 390 1–2 8391 .

    • Crossref
    • Search Google Scholar
    • Export Citation
  • 18. Gao, M, Ling, BC, Yang, SS, Zhao, M. Flame retardance of wood treated with guanidine compounds characterized by thermal degradation behavior. J Anal Appl Pyrolysis 2005 73:151156 .

    • Crossref
    • Search Google Scholar
    • Export Citation
  • 19. Qingfeng, L, Chunxiang, L, Yonggang, Y, Fu, H, Licheng, L. Investigation on the effects of fire retardants on the thermal decomposition of wood-derived rayon fiber in an inert atmosphere by thermogravimetry–mass spectrometry. Thermochim Acta 2004 419:205209 .

    • Crossref
    • Search Google Scholar
    • Export Citation
  • 20. Pappa, A, Mikedi, K, Tzamtzis, N, Statheropoulos, M. Chemometric methods for studying the effects of chemicals on cellulose pyrolysis by thermogravimetry–mass spectrometry. J Anal Appl Pyrolysis 2003 67 2 221235 .

    • Crossref
    • Search Google Scholar
    • Export Citation
  • Collapse
  • Expand

To see the editorial board, please visit the website of Springer Nature.

Manuscript Submission: HERE

For subscription options, please visit the website of Springer Nature.

Journal of Thermal Analysis and Calorimetry
Language English
Size A4
Year of
Foundation
1969
Volumes
per Year
1
Issues
per Year
24
Founder Akadémiai Kiadó
Founder's
Address
H-1117 Budapest, Hungary 1516 Budapest, PO Box 245.
Publisher Akadémiai Kiadó
Springer Nature Switzerland AG
Publisher's
Address
H-1117 Budapest, Hungary 1516 Budapest, PO Box 245.
CH-6330 Cham, Switzerland Gewerbestrasse 11.
Responsible
Publisher
Chief Executive Officer, Akadémiai Kiadó
ISSN 1388-6150 (Print)
ISSN 1588-2926 (Online)

Monthly Content Usage

Abstract Views Full Text Views PDF Downloads
Jun 2023 5 0 0
Jul 2023 1 0 0
Aug 2023 15 1 2
Sep 2023 8 0 0
Oct 2023 3 4 0
Nov 2023 7 3 0
Dec 2023 0 0 0