electrode. The PVA/β-CD nanofibers were continuously collected until 2.5 h. After the electrospinning, nanofibers were exposed to HCl fumes for 1 min to convert into crosslinked PVA/β-CD nanofibers. ‘Water solubility test’ was used to check nanofiber